Fair Shine industrial (Hong Kong) Co., Limited 
Home > Surface Treatment

Burnt blue

2024-09-28 13:51:31

1727502685349300

After the entire carcass is filled with colored glaze, it is then baked in a blast furnace with a furnace temperature of about 800°C. The colored glaze melts from a sandy solid to a liquid, and after cooling, it becomes a gorgeous colored glaze that is fixed on the carcass. When the color glaze is lower than the height of the copper wire, it must be filled with the color glaze again and then fired, usually four or five times in a row until the pattern is filled in to be level with the filigree pattern.

Previous: Shot Peening 2024-09-28
Next: Brushed metal 2024-09-28

Fair Shine industrial (Hong Kong) Co., Limited

To provide customers with the most comprehensive precision mold parts solutions.

+86 189 2682 6341

Block 1, No. 12, Wusong 4th Street, Yuwu Industrial Zone, Dongcheng District, Dongguan, Guangdong, China

Get A Quote
  • Please enter your name.
  • Please enter your E-mail.
  • Please enter your Phone or WhatsApp.
  • Please refresh this page and enter again
    The message requires at least 20 characters.